Sustainability-oriented machining of additively manufactured SS316L: Impact of laser powder bed fusing process parameters under MQL milling


Khan A. M., Ali M. A., Waqar S., Jamil M., KAYNAK Y., Zhao G.

Journal of Manufacturing Processes, cilt.170, ss.80-105, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 170
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1016/j.jmapro.2026.05.008
  • Dergi Adı: Journal of Manufacturing Processes
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, ABI/INFORM, Compendex, INSPEC
  • Sayfa Sayıları: ss.80-105
  • Anahtar Kelimeler: Carbon emissions, Energy consumption, Laser powder bed fusing, MQL milling, Surface integrity, Sustainability, Tool wear
  • Marmara Üniversitesi Adresli: Evet

Özet

This work presents a detailed investigation of machinability behavior of Laser Powder Bed Fusing (LPBF) SS316L when machined using Minimum Quantity Lubrication (MQL) milling with specific focus on the interactions among cutting speed (60, 80, 120 m/min), feed per tooth (0.02, 0.04, 0.06 mm/tooth), scanning strategies (unidirectional, strip and island), and build layer rotation angles (0°, 45° and 90°). The analysis covered surface integrity, tool wear behavior, tool life, the material removal volume (MRV), power usage, energy efficiency, and carbon emission, thus enabling a combined productivity sustainability analysis. The findings illustrate that surface roughness and integrity are highly sensitive to feed and cutting speed, and low feed per tooth (0.02 mm/tooth), and moderate cutting speed (60–80 m/min) produced consistently smooth and uniform surfaces with minimal tearing and adhesive deposition. Thermo-mechanical loading increased substantially with an increase in feed to 0.06 mm/tooth and cutting speed to 120 m/min resulting in deeper feed marks as well as smearing and adhesion layers. The rate of tool wear also increased significantly under aggressive machining; at a constant cutting speed (100 m/min) tool life decreased to 14.9, 13.01, and 11.05 min (unidirectional, island, and strip respectively) as the feed increased to 0.06 mm/tooth. Similarly, at a constant feed (0.04 mm/tooth) increasing the cutting speed from 60 to 120 m/min reduced tool life from 15.5 min to approximately 7 min, and productivity measured in terms of MRV decreased from 12,070 mm3 at 60 m/min to 5300 mm3 at 120 m/min; strip scanning produced steeper and more stable walls compared with island scanning, and 45 and 90 degrees rotation of the tool face greatly increased chip evacuation and reduced the anisotropic resistance. Consequently, under harsh environments, there was high energy usage and emissions whereas under moderate regimes of cutting, they were reduced. Overall, the best machining performance was achieved at feeds of 0.02–0.04 mm/tooth, cutting speed of 60–80 m/min, strip/island scanning, and 45- or 90-degree rotation of layers, which substantiates their performance in providing technically sound, energy-saving, and environmental-friendly machining of SS316L fabricated by LPBF at MQL conditions.