MATERIALS LETTERS, cilt.60, ss.2207-2210, 2006 (SCI-Expanded)
This article reports the mechanical properties, the microstructure, and the crystallography of composite materials made of hydroxyapatite, obtained from natural bovine bone, and TiO2 (5 and 10 wt.%), which were sintered at different temperatures between 1000 and 1300 degrees C. Higher sintering temperatures resulted in better densification. The samples sintered at 1300 degrees C had the highest microhardness. The best compressive strengths were obtained after sintering at 1300 degrees C for the samples containing 5% TiO2, and at 1200 degrees C for the samples with 10% TiO2. (c) 2005 Elsevier B.V. All rights reserved.