INCREASING THE SURFACE PROPERTIES OF THE WIDELY USED AISI4140 STEEL BY COATING WITH CO-BASED SUPERALLOY BY LMD METHOD


ÖNER A., YALÇINKAYA S.

6.ULUSLARARASI MÜHENDİSLİK VE TEKNOLOJİ YÖNETİMİ KONGRESİ, İstanbul, Turkey, 21 November 2021, vol.6, pp.599-560

  • Publication Type: Conference Paper / Summary Text
  • Volume: 6
  • City: İstanbul
  • Country: Turkey
  • Page Numbers: pp.599-560