INCREASING THE WEAR PROPERTIES AGAINST HIGH TEMPERATURE BY COATING THE IRON-BASED SUPERALLOY TO 4140 STEEL BY LASER MELTING DEPOSITION METHOD


YALÇINKAYA S. , ÖNER A.

6th INTERNATIONAL CONGRESS ON ENGINEERING AND TECHNOLOGY MANAGEMENT, İstanbul, Turkey, 20 - 21 November 2021, vol.6

  • Publication Type: Conference Paper / Summary Text
  • Volume: 6
  • City: İstanbul
  • Country: Turkey